Growth and crystallization of titanium anodized films were studied by performing the anodization of the sputter-deposited titanium samples under cyclic voltammetry (CV) mode at very low potentials. The surface features, crystalline behaviors and chemical compositions of the formed anodic oxide layers were detected by AFM, SE and XPS. It was found that the structure of the titanium anodized films is crystalline, even though the maximum oxidation potential (ϕmax) is very low (as low as 1000 mV). Both enlarging the applied voltage and reducing the potential scanning rate are beneficial for the growth and crystallization of titanium oxide films. It was thought that the internal compressive stress, other than the local joule heating accepted for many researchers, is the main force of stimulating the crystallization of anodic titanium oxide films at very low potentials.

影响因子
1.342
论文下载
作者

Jun-heng XING,Zheng-bin XIA,Hui LI,Ying-ying WANG,Li ZHONG.

期刊

Trans.Nonferrous Met.Soc.China,23,3286−3292(2013)